MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Online Metals
Visit Online Metals for fast service
on small quantity orders.
ExxonMobil EXACT™ 8203 Octene-1 Plastomer  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Ethylene based octene plastomer produced in a solution polymerization process using a metallocene catalyst. Designed for applications requiring high flexibility, outstanding toughness, excellent low temperature flex-cracking resistance and high clarity. This material combines favorable melt strength with an excellent processability, offering important advantages for foam, wire and cable and extrusion applications. Suitable for improving the impact resistance or flexibility of molded polyolefins.

Information provided by ExxonMobil Chemical

Vendors:
Available Properties
  • Density, ISO 1183
  • Mooney Viscosity, ASTM D1646, ML (1 + 4)
  • Environmental Stress Crack Resistance, ASTM D1693
  • Thickness
  • Melt Flow, ISO 1133
  • Hardness, Shore A, ISO 868, 15s
  • Hardness, Shore D, ISO 868, 15s
  • Tensile Strength at Break, ISO 527-2
  • Elongation at Break
  • Flexural Modulus, ISO 178
  • Izod Impact, Notched, ASTM D256
  • Izod Impact, Notched, ASTM D256
  • Impact, Internal Method, Puncture resistance max. tension, MPa
  • Impact, Internal Method, Puncture Resistance Energy, MJ/mm
  • Dart Drop, ASTM D4272
  • 1% Secant Modulus, MD, ASTM D882
  • 1% Secant Modulus, TD, ASTM D882
  • Heat Seal Strength Initiation Temperature, Internal Method
  • Heat of Fusion, ASTM D3418, DSC
  • Melting Point, ASTM D3418, DSC peak melting point
  • Vicat Softening Point, ISO 306, at 10 N
  • Brittleness Temperature, ASTM D746
  • Haze, ASTM D1003
  • Gloss, ASTM D2457
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Exxon Chemical

Category Notes
Plastic
Thermoplastic Elastomer

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2026 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.