MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Eastman Cadence™ GS5 Clear (Unpigmented) Copolyester for film calendering
Categories: Polymer; Film; Thermoplastic; Polyester, TP; Polyester Film

Material Notes: Cadence™ GS5 is an amorphous copolyester with improved processability for film calendering. Calendered films made of Cadence™ copolyester are non-crystallizing, are halogen-free, offer wide calendering and thermoforming windows and have good low-temperature toughness. They are cooperative in secondary operations such as solvent-bonding, lamination, decoration, cold-forming, punching/cutting and embossment. Eastman Cadence™ resins require no pre-drying or additional stabilizers. This product has been GREENGUARD INDOOR AIR QUALITY CERTIFIED®.

Application/Uses

  • Appliance films
  • Architectural laminates
  • Automotive films
  • Bags
  • Decorative laminates
  • Electronic laminates
  • Floor coverings
  • Furniture/Furniture trim
  • Labels
  • Outdoor films
  • Packaging
  • Printable films
  • Shrink film
  • Transaction cards
  • Transportation laminates
  • Wall coverings

Reported typical properties are preliminary. Information was provided by Eastman.

Vendors:
Available Properties
  • Specific Gravity, ASTM D792
  • Hardness, Shore A, ASTM D2240
  • Secant Modulus, MD, ASTM D882, Tangent
  • Secant Modulus, TD, ASTM D882, Tangent
  • Film Tensile Strength at Break, MD, ASTM D882
  • Film Tensile Strength at Break, TD, ASTM D882
  • 1% Secant Modulus, MD, ASTM D882
  • 1% Secant Modulus, TD, ASTM D882
  • Brittleness Temperature, ASTM D1790, by Impact
  • Transmission, Visible, clear; thickness not quantified
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Eastman Chemical Company

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.