MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Dow Elvaloy® 2116 AC Ethylene and 16% Ethyl Acrylate Copolymer
Categories: Polymer; Film; Thermoplastic

Material Notes: Elvaloy® 2116 AC is intended for profile and tube extrusion. Its good chemical resistance, low temperature toughness and good flex life make it outstanding for specialty tubing. The material also is recommended for contour extrusion and for blow molding of toys, gaskets and other parts requiring permanent flexibility, stress cracking resistance and low temperature toughness. Elvaloy® 2116 AC also can be used in film applications where softness and flexibility are needed.

Elvaloy® 2116 AC is easily processed on standard equipment used for low density polyethylene. It is very heat stable and does not give corrosive decomposition products during processing, even at the upper limit of the recommended temperature range.

Information provided by DuPont.

This former DuPont product line is now a Dow product line.

Vendors:
Available Properties
  • Density, ASTM D792 - ISO 1183
  • Melt Flow, ASTM D1238 - ISO 1133
  • Hardness, Shore A, ASTM D2240 - ISO 868
  • Hardness, Shore D, ASTM D2240 - ISO 868
  • Tensile Strength at Break, ASTM D638 - ISO 527-2, 500 mm/min
  • Elongation at Break, ASTM D638 - ISO 527-2, 500 mm/min
  • Tensile Modulus, ASTM D638 - ISO 527-2, 1 mm/min
  • Melting Point, ASTM D3418 - ISO 3146, By DSC
  • Vicat Softening Point, ASTM D1525 - ISO 306, A50 (10N)
  • Rear Barrel Temperature, Extrusion lamination and extrusion coating
  • Rear Barrel Temperature, Cast film
  • Rear Barrel Temperature, Blown film
  • Middle Barrel Temperature, Blown film
  • Middle Barrel Temperature, Cast film
  • Middle Barrel Temperature, Extrusion lamination
  • Front Barrel Temperature, Blown film
  • Front Barrel Temperature, Cast film
  • Front Barrel Temperature, Extrusion lamination
  • Adapter Temperature, Blown film
  • Adapter Temperature, Cast Film
  • Adapter Temperature, Extrusion lamination
  • Die Temperature, Blown film
  • Die Temperature, Cast film
  • Die Temperature, Extrusion lamination
  • Melt Temperature, For blow molding
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Dow Chemical (former DuPont)

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.