MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Specialty Compounds RTP Company
Bohler-Uddeholm UDDEHOLM RAMAX® S Modified 420F  (discontinued **)
Categories: Metal; Ferrous Metal; Stainless Steel

Material Notes: Chromium alloyed stainless holder steel

A pre-hardened stainless holder steel with excellent machinability, high tensile strength and good corrosion resistance.

RAMAX® S is characterized by:

  • Excellent machinability
  • Good corrosion resistance
  • Uniform hardness in all directions
  • Good indentation resistance

Applications:

  • Holders/bolsters for plastic molds. RAMAX S in combination with STAVAX ESR or ELMAX as insert material gives a completely corrosion resistant mold.
  • Plastic and rubber molds with low requirements on polishability.
  • Dies and callipers for plastic extrusion.
  • Constructional parts

Key Words: AISI 420F
Vendors:
Available Properties
  • Density, hardened and tempered to 340 HB
  • Density, hardened and tempered to 340 HB
  • Hardness, Brinell, Hardened and tempered (Delivery condition)
  • Hardness, Brinell, tempering temp 200-1200°F
  • Tensile Strength, Ultimate, (hardened to 340 HB)
  • Tensile Strength, Ultimate, (hardened to 340 HB)
  • Tensile Strength, Yield, 68°F (hardened to 340 HB)
  • Tensile Strength, Yield, hardened to 340 HB
  • Elongation at Break, (hardened to 340 HB)
  • Elongation at Break, hardened to 340 HB
  • Reduction of Area, hardened to 340 HB
  • Reduction of Area, hardened to 340 HB
  • Modulus of Elasticity, 68°F, (hardened and tempered to 340 HB)
  • Modulus of Elasticity, hardened and tempered to 340 HB
  • Impact Test, hardened and tempered to 340 HB
  • Impact Test, hardened and tempered to 340 HB
  • CTE, linear, hardened and tempered to 340 HB
  • Specific Heat Capacity, hardened and tempered to 340 HB
  • Thermal Conductivity, hardened and tempered to 340 HB
  • Carbon, C
  • Chromium, Cr
  • Iron, Fe, as balance
  • Manganese, Mn
  • Silicon, Si
  • Sulfur, S
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

New MatWeb Services
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.