| KEBABLEND / M FE 151101 is a development product based on PA12 for the production of injection molded magnets. Due to the high degree of filling with anisotropic rare earths, KEBABLEND /M FE 151101 enables the injection molding of very high-performance magnets. Properties: dimensionally stable, magnetizable, semi-crystalline Typical areas of application: Magnets for sensors, Pumps and motors Industries: Automotive, Electrical and electronics industry, Household appliances, Mechanical Engineering, Sanitary industry Information provided by BARLOG plastics GmbH. |