MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Metal adhesives
Zyvex Performance Materials Epovex™ HK-100 Carbon Nanotube Two-Part Epoxy Adhesive  (discontinued **)
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive, Flexible

Material Notes: HK-100 is a carbon nanotube enhanced ambient or elevated temperature cure two-part epoxy adhesive. Used for bonding, laminating, filling or potting, HK-100 is ideal for many metals, woods, masonry products, and some plastics and rubbers. HK-100 was also designed to bond Zyvex Performance Material’s Arovex composites. Additional fillers or glass micro-beads may be added to control sag qualities or to control bond-line thickness to a specific specification.

HK-100 exhibits excellent flexibility, very high T-peel strength, and very high tensile shear strength.

Vendors:
Available Properties
  • Specific Gravity, Part B, uncured
  • Specific Gravity, Blend, uncured
  • Specific Gravity, Part A, uncured
  • Viscosity, Part B, uncured
  • Viscosity, Blend, uncured
  • Viscosity, Part A, uncured
  • Adhesive Bond Strength, 75°F/7 day cure; vs. acid etched 6061-T6 Aluminum
  • Adhesive Bond Strength, 75°F/7 day cure; vs. acid etched 6061-T6 Aluminum
  • Adhesive Bond Strength, 75°F/7 day cure; vs. acid etched 6061-T6 Aluminum
  • Adhesive Bond Strength, 176°F/2 hr Cure; vs. acid etched 6061-T6 Aluminum
  • Peel Strength, 75°F/1 day cure
  • Peel Strength, 75°F/12 hr + 176°F/ 1hr cure
  • Peel Strength, 75°F/3 day cure
  • Cure Time, for max strength
  • Cure Time, full strength not reached until after 7 days at RT
  • Pot Life
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Zyvex Performance Materials (ZPM)

Category Notes
Plastic

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Metal adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.