| HB0976 is a pelleted high molecular weight, high density polyethylene Hexene-1 resin for blow molding. HB0976 meets the U.S. Food and Drug Administration (FDA) criteria for food contact use as specified in 21 CFR 177.1520 (c) 3.1a & 3.2a. Applications: Large size shipping containers and drums, household and industrial chemical containers, toiletries and cosmetic containers. Advantages: Excellent stress crack resistance, excellent resistance to most chemicals and outstanding rigidity with balanced impact strength and stiffness, high melt strength and moderate die swell. Information provided by Lotte Advanced Materials. |