MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
General Plastics LAST-A-FOAM® FR-4615 Foam
Categories: Other Engineering Material

Material Notes: Product Description: The LAST-A-FOAM®FR-4600 Microcell Series supports the most intricate detail while eliminating extra prep work. With an even-smoother surface finish than our LAST-A-FOAM® FR-4500 material, they are superb for prototypes and models, and precision tooling applications. Advanced microcell technology creates a grain-free, ultra smooth exterior for painted finishes, significantly reducing process time. What’s more, its finer cell structure is comparable to higher-density foam products without the added cost and weight.

Key Performance Benefits:

  • Ultra smooth finish
  • Lighter, less abrasive than syntactic boards
  • Creates intricate, 3-D details
  • Dimensionally stable
  • Special formulation allows creation of shavings when material is machined
  • Reduced cutting tool abrasion
  • Large sheets up to 60” x 120”
Applications:
  • 3-D Signage
  • Design prototypes
  • Appearance or “sight” models
  • Architectural models
  • Topographical maps
  • Tooling and molds for low temperature curing prepregs (<200ºF)
  • Decorative moldings

Information provided by General Plastics Manufacturing Company

Vendors:
Available Properties
  • Density, ASTM D1622
  • Hardness, Shore D, ASTM D2240
  • Tensile Strength, ASTM D1623, Perpendicular to Rise
  • Flexural Strength, ASTM D790
  • Flexural Strength, ASTM D790, Rise Parallel to Beam Thick.
  • Flexural Strength, ASTM D790, Rise Parallel to Test Span
  • Flexural Modulus, ASTM D790
  • Flexural Modulus, ASTM D790 Method 1-A, Rise Parallel to Beam Thick.
  • Flexural Modulus, ASTM D790 Method 1-A, Rise Parallel to Test Span
  • Compressive Strength, ASTM D1621, Parallel to Rise
  • Compressive Strength, ASTM D1621, Perpendicular to Rise
  • Compressive Strength, ASTM D1621, Parallel to Rise
  • Compressive Strength, ASTM D1621, Perpendicular to Rise
  • Compressive Modulus, ASTM D1621, Parallel to Rise
  • Compressive Modulus, ASTM D1621, Perpendicular to Rise
  • Compressive Modulus, ASTM D1621, Perpendicular to Rise
  • Compressive Modulus, ASTM D1621, Parallel to Rise
  • Shear Modulus, ASTM C273, Rise Parallel to Specimen Thickness
  • Shear Strength, ASTM C273, Rise Parallel to Specimen Thickness
  • CTE, linear, GP Method
  • Thermal Conductivity, ASTM C518
  • Glass Transition Temp, Tg, ASTM E1824
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.