| DuPure ST 77 A is a heterophasic copolymer (produced with a phthalate-free catalyst), suitable for injection molding applications. The product is nucleated and contains an anti-electrostatic agent, good flowability and a good balance of stiffness and impact strength. Applications: DuPure ST 77 A is suitable for: general injection molding, packaging. Information provided by Ducor Petrochemicals |