MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Phillips 66 Wireline ISO Grade 680
Categories: Fluid; Lubricant

Material Notes: Wireline is a high-quality, tacky, viscous, high viscosity index lubricant specifically developed for lubrication and sealing of braided wirelines and cables used in oil and gas wells for cased-hole logging, pipe recovery service, tubing conveyed perforating, production logging and reservoir analysis. Wireline is applied in once-through operation. It maintains a seal around the moving wireline in high-pressure environments to prevent the escape of wellbore corrosive fluids and gases between the wireline outer diameter and the flow tube inner diameter. It provides excellent protection against corrosion, including saltwater corrosion, as well as rust preventive properties for storage of logging cables. It also has excellent low-temperature fluidity to prevent wireline seizure and breakage in cold weather. Wireline passes the visual “no sheen” requirements of the U.S. EPA/U.S. Coast Guard Static Sheen Test (Federal Register Vol. 58, No.41).

Applications:

  • Braided wirelines and cables used in oil & gas wells
  • Cased-hole logging operations
  • Pipe recovery service
  • Tubing-conveyed perforating
  • Production logging
  • Reservoir analysis
Features/Benefits:
  • Clear color
  • Easy to apply in warm and cold weather
  • Tacky; stays put and does not drip
  • Excellent corrosion protection
  • Excellent low-temperature fluidity
  • High viscosity index
  • Easily pumpable in wireline injection units
  • Inherently biodegradable

Information provided by Phillips 66 Lubricants.

Vendors:
Available Properties
  • Specific Gravity
  • Density
  • Viscosity Measurement, Index
  • Kinematic Viscosity at 40°C (104°F)
  • Kinematic Viscosity at 100°C (212°F)
  • ASTM Color, ASTM D1500
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Pour Point
  • Flash Point, COC
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.