MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Versalis Clearflex® H&T FGH 196 Hexene Copolymer Linear Low Density Polyethylene
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Film Grade; LLDPE/Hexene, Film Grade

Material Notes: Clearflex H&T FGH 196 is a hexene copolymer linear low density polyethylene (C6-LLDPE), with antioxidants and processing aid, suitable for blown film extrusion.

Films obtained from Clearflex H&T FGH 196 show excellent optical properties, a wide sealing window, both hot tack and heat seal, together with a low sealing initiation temperature (S.I.T.) and outstanding impact, puncture and Elmendorf tear resistance.

Main Applications: Clearflex H&T FGH 196, for its overall characteristics, is the right choice for all applications, like silage stretch film, low thickness high clarity packaging film, requiring a superior mechanical strength. Moreover, the excellent sealability behavior makes it ideal for lamination film production.

Information provided by Polimeri Europa.

Versalis is the Eni subsidiary containing the plastics and rubber businesses.

Vendors:
Available Properties
  • Specific Gravity, ISO 1183
  • Thickness, Recommended
  • Melt Flow, ISO 1133
  • Film Tensile Strength at Yield, MD, ISO 527-3
  • Film Tensile Strength at Yield, TD, ISO 527-3
  • Film Elongation at Break, MD, ISO 527-3
  • Film Elongation at Break, TD, ISO 527-3
  • Coefficient of Friction, Dynamic, ISO 8295
  • Elmendorf Tear Strength, MD, ISO 6383-2
  • Elmendorf Tear Strength, TD, ISO 6383-2
  • Dart Drop Test, ISO 7765-1, F50
  • Film Tensile Strength at Break, MD, ISO 527-3
  • Film Tensile Strength at Break, TD, ISO 527-3
  • 1% Secant Modulus, MD, ISO 527-3
  • 1% Secant Modulus, TD, ISO 527-3
  • Melting Point, Internal method
  • Vicat Softening Point, ISO 306/A
  • Brittleness Temperature, ASTM D746
  • Haze, ISO 14782
  • Gloss, ASTM D2457, 45°
  • Transmission, Visible, clear; thickness not quantified
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Polimeri Europa (Former Polimeri Europa (EniChem)

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.