| Description: Cosmic EH51 is an iron-filled epoxy molding compound which is supplied in a black granular form. Features: This material flows easily under low pressure and provides good moldability. Applications: This material is good for EMI / RFI shielding, and can be either compression or transfer molded to fabricate core rods, or to encapsulate surface mount and axial leaded inductors. This single molded compound eliminates the labor intensive over/under molding. Test Conditions: 1 MHz; 1/16" Rod; 0.008" wire; 25 No. of Turns Data provided by the manufacturer. |