MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Eastman Saflex® RA41/RB41 Clear PVB interlayer
Categories: Polymer; Film

Material Notes: Saflex® Clear PVB interlayer, our most popular formulation, is available in two different adhesion levels for architectural applications. These different adhesion levels are generally selected based on the laminator’s processing parameters. Both formulations give architects and builders the ability to meet or exceed the human safety impact requirements for laminated safety glass with properly produced laminates.
  • Protects building occupants and pedestrians from flying and falling glass shards after accidental breakage
  • Provides security through burglary and forced-entry resistance and ballistics and bomb blast protection
  • Provides severe windstorm and debris-impact resistance
  • Reduces the transmission of unwanted sound into a building’s environment or between walls
Applications:
Interior: Partitions, doors, windows, skylights, furniture, balustrades, retail shelving, flooring
Exterior: Doors, windows, curtain walls, wall coverings, and overhead glazing

Information provided by Eastman

Vendors:
Available Properties
  • Density, ASTM D792
  • Hardness, Shore D, ASTM D2240, Cut/stacked to 12.5 mm
  • Tensile Strength at Break, ISO 527-3
  • Elongation at Break, ISO 527-3
  • Modulus of Elasticity, 3 sec
  • Poissons Ratio, ASTM D638, 50% RH
  • Shear Modulus, 3 sec
  • CTE, linear, ASTM D831
  • Specific Heat Capacity, ASTM E1269
  • Thermal Conductivity, ASTM F433
  • Refractive Index, ASTM D542
  • Haze, ASTM D1003, clear
  • Yellow Index, ASTM E313, 3-mm clear
  • Transmission, Visible, NFRC 300, ISO 9050, EN410, Solar, 3-mm clear
  • Transmission, Visible, NFRC 300, ISO 9050, EN410, Visible, 3-mm clear
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Eastman Chemical Company

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.