MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Dow Nucrel® 699 Ethylene-Methacrylic Acid Copolymer Resin
Categories: Polymer; Thermoplastic; Ethylene Methyl Acrylate

Material Notes: Nucrel® 599 is a tough, lightweight, easily processed ethylene copolymer resin. This resin is inherently flexible without the need for plasticizers. The resin can be pigmented, UV-stabilized for exterior applications and painted or plated for special decorative effects.

Typical Applications:

  • Ink modification
  • Adhesive component
  • Special adhesive films

Features:

  • Higher deflection temperature
  • Good adhesion to metals and polar substrates

Information provided by DuPont.

This former DuPont product line is now a Dow product line.

Vendors:
Available Properties
  • Density, ASTM D792
  • Melt Index of Compound, ASTM D1238
  • Hardness, Shore D, ASTM D2240, Initial (peak) hardness
  • Tensile Strength at Break, ASTM D638, Type IV specimen, compression molded, crosshead speed 2 in/min
  • Elongation at Break, ASTM D638, Type IV specimen, compression molded, crosshead speed 2 in/min
  • Flexural Modulus, ASTM D790
  • Izod Impact, Notched, ASTM D256
  • Tensile Impact Strength, ASTM D1822S
  • Tensile Impact Strength, ASTM D1822S
  • Melting Point, ASTM D3418(DSC)
  • Vicat Softening Point, ASTM D1525
  • Zone 1
  • Zone 2
  • Zone 3
  • Zone 4
  • Zone 5
  • Die Temperature
  • Melt Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Dow Chemical (former DuPont)

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.