MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
ExxonMobil 222 Special Mobilgrease XHP Series
Categories: Fluid; Lubricant; Lithium Gellant

Material Notes: Mobilgrease XHP Series products are extra high performance lithium complex greases intended for a wide variety of applications and severe operating conditions. These greases were designed to outperform conventional products by applying leading edge, proprietary, lithium complex manufacturing technology. They are based on high quality paraffinic mineral oils and are manufactured and formulated to provide excellent high temperature performance with good adhesion, structural stability and resistance to water contamination. These greases have a high level of chemical stability and offer excellent protection against rust and corrosion. The greases feature high dropping points and maximum recommended operating temperature for the Series is 175°C.

Mobilgrease XHP greases are used in a wide range of equipment including industrial, automotive, construction and marine applications: Mobilgrease XHP 222 is recommended for industrial and automotive antifriction bearings, chassis components, universal joints and disc brake wheel bearings. It finds particular application in passenger cars, light trucks, taxi fleets and farm equipment. It is also recommended for marine, paper mill, sugar mill and mining applications; Mobilgrease XHP 461 is recommended for construction and mining equipment, paper and steel mills and other heavy-duty applications; Mobilgrease XHP 222 Special is used in chassis components, clutch bearings, ball joints of suspension and steering systems in all kinds of passenger cars, trucks, farm tractors, contractor, construction, earth-moving, and mobile equipment. Contains molybolenum disulphide that provides protection from wear under shock loads and fretting conditions.

Key Words: NLGI Grade 2
Vendors:
Available Properties
  • Kinematic Viscosity at 40°C (104°F), ASTM D445
  • Oxidative Stability, ASTM D942, Pressure Drop of 35 kPa
  • Four Ball Extreme Pressure, Weld Load, ASTM D2596
  • Four Ball Wear, ASTM D2266
  • Penetration, ASTM D1831, Penetration Consistency Change, Roll Stability, mm/10
  • Penetration, ASTM D217, Worked, 25°C
  • Timken Test
  • Dropping Point, ASTM D2265
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

New MatWeb Services
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.