MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Colmant Coated Fabrics CR (NEOPRENE®) Coated Cotton Fabric
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Neoprene coated cotton fabric combines my following properties: Neoprene has a very good resistance to water, cold oils, aging and chemicals. It has a good resistance to sunlight and badweather. Neoprene has good mechanical properties. Neoprene® has excellent flame resistance.
Limitations: It has low gas permeability and average electrical performance. Cotton is a natural fiber of vegetable origin. The cotton thread is derived from the transformation of the hair of the Gossypium (or cotton plant). We also designate under the same name the fabric resulting from the weaving of this thread. Cotton is the first textile fiber used in the world despite the advent of synthetic fibers. Flammable. It decomposes around 160°C. Cotton is popular thanks to its characteristics: appearance, lightness, comfort and ease of assembly and transformation.

Applications:

  • Industrial fabrics
  • straps
  • tarps
  • tires
  • rope
  • clothing
  • protective bellows
  • inflatables
  • CBRN suits
  • thermic insulation combinations
Properties:
  • Fireproofed
  • Acids resistance
  • Non-skid
  • UV resistance
  • Water resistance
  • Airtightness
  • Isolation to radiation

Information provided by COLMANT COATED FABRICS

Vendors:
Available Properties
  • Hardness, Shore A
  • Tensile Strength at Break
  • Elongation at Break
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.