| TPE-S, Shore A65, translucent. Abrasion resistant, high dynamic load capacity, good DVR and good adhesion to PP in 2K injection molding. Properties: flexible, good haptics, good recovery behavior, High wear resistance, semi-crystalline, soft Typical areas of application: Sealing elements, Seals, Handles, Haptic components, Rollers, Hoses, Sports & Leisure Articles Industries: Automotive, Electrical and electronics industry, Household appliances, Industry, Mechanical Engineering, Furniture industry, Sports & Recreation Information provided by BARLOG plastics GmbH. |