MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Reynolds OOMOO® 30 Tin Cure Silicone Rubber
Categories: Polymer; Thermoset; Silicone; Silicone Rubber

Material Notes: Product Overview: No Vacuuming – No Scale – Easy To Use . . . OOMOO™ 25 & 30 are easy to use tin cure silicone rubber compounds that feature convenient one-to-one by volume mix ratios (no scale necessary). Both have low viscosities for easy mixing and pouring . . . vacuum degassing is not necessary. Both products cure at room temperature with negligible shrinkage. OOMOO™ 30 has a 30-minute pot life, with a six-hour cure time. OOMOO™ 25 is a faster version, with a 15-minute pot life and 75 minute cure time. For The Novice Mold Maker - OOMOO™ silicones do not have great tear strength. They are good for making simple one- or two-piece block molds. If you require a high-tear strength silicone, Mold Max™ silicones are recommended. More information on Mold Max™ silicones is available at www.smooth-on.com. OOMOO™ 25 & 30 are suitable for a variety of art-related and industrial applications including making one and two-piece block molds for sculpture and prototype reproduction, casting plaster, resins and wax. OOMOO™ silicones are also suitable for electrical potting and encapsulation applications.

Information provided by Reynolds Advanced Materials

Vendors:
Available Properties
  • Specific Gravity, ASTM D-1475
  • Viscosity, ASTM D-2393, Mixed
  • Linear Mold Shrinkage, ASTM D-2566
  • Hardness, Shore A, ASTM D-2240
  • Tensile Strength, ASTM D-412
  • Elongation at Break, ASTM D-412
  • 100% Modulus, ASTM D-412
  • Tear Strength, ASTM D-624, Die C
  • Volume Resistivity, ASTM D-150-98
  • Surface Resistance, ASTM D-150-98
  • Dielectric Constant, ASTM D-150-98
  • Dielectric Strength, ASTM D149
  • Dissipation Factor, ASTM D-150-98
  • CTE, linear, ASTM E-831-06
  • Thermal Conductivity, ASTM D-1461
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Cure Time
  • Pot Life, ASTM D-2471
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.