MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Wolf Kunststoff ZEDEX® ZX-100K 3D Polymer
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer

Material Notes: Description: In addition to the very good tribological properties, such as very low wear and good friction values, ZX-100K tribofilaments offer universal properties. Due to the universal properties, it can be used in a variety of ways. ZX-100K tribofilaments are not brittle, do not warp and can be used for large components. ZX-100K Tribofilaments have an approval for permanent contact with foodstuffs and the printing is odorless. Depending on the printing parameters, it can be printed in mother-of-pearl colour.

Characteristics

  • Hard, stiff, tough but at the same time elastic
  • Good weathering resistance
  • Good machinability
  • Bondable and weldable
  • PTFE and silicon free
  • Low-outgassing
  • Support material easy to detach
  • Food industry conform
  • Affordable price
Conformities
  • LABS
  • KTW
  • FDA & EU 10/2011

Information provided by Zedex

Vendors:
Available Properties
  • Tensile Strength at Break, DIN EN ISO 527-2/1B/5, XY (flat)
  • Tensile Strength, DIN EN ISO 527-2/1B/5, XY (flat)
  • Tensile Strength, Yield, DIN EN ISO 527-2/1B/5, XY (flat)
  • Elongation at Break, DIN EN ISO 527-2/1B/5, XY (flat)
  • Elongation at Break, DIN EN ISO 527-2/1B/5, XY (flat), at tensile strength
  • Elongation at Yield, DIN EN ISO 527-2/1B/5, XY (flat)
  • Tensile Modulus, DIN EN ISO 527-2/1B/1, XY (flat)
  • Charpy Impact Unnotched, DIN EN ISO 179
  • Deflection Temperature at 1.8 MPa (264 psi), DIN EN ISO 75
  • Shrinkage, Annealing, thickness
  • Shrinkage, Annealing, length
  • Shrinkage, Annealing, width
  • Nozzle Temperature
  • Moisture Content, DIN EN ISO 15512, Filament moisture content during printing
  • FDA
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.