Pro-fax SV258 impact polypropylene copolymer is available in pellet form. This resin is typically used in extrusion applications and offers very good cold temperature impact resistance. Availability: North America Application: Automotive Parts; Corrugated Sheet; Opaque Containers Market: Rigid Packaging Processing Method: Compounding; Extrusion Blow Molding; Sheet; Sheet and Profile Extrusion; Thermoforming Attribute: Good Dimensional Stability; Good Stiffness; Low Temperature Impact Resistance Information provided by LyondellBasell. |