MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Zircar Refractory Composites RS-200 Refractory Sheet
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes: ZRCI Refractory Sheet Type RS-200 is a fiber-reinforced ceramic laminate with useful properties to 1260°C (2300°F). This high temperature product offers high strength, moderate thermal conductivity and excellent electrical insulation. It retains its strength and utility to levels far exceeding maximum use temperatures of reinforced plastics and asbestos cement replacements. RS-200 is 100% inorganic, non-flammable and contains no asbestos. Its high alumina content makes it resistant to many environments including molten aluminum. RS-200 undergoes little or no outgassing on heating, is not brittle, and may be cut and machined with standard tooling. RS-200 is available in standard and custom boards and is useful as Specialty Furnace Components, Specialty High Temperature Electrical Thermal Insulation, Metal Working Components and Induction Furnace Components.

Information provided by ZIRCAR Refractory Composites, Inc. (ZRCI)

Vendors:
Available Properties
  • Density
  • Porosity
  • Modulus of Rupture
  • Modulus of Rupture
  • Modulus of Rupture
  • Compressive Strength, 24 hrs at 510°C, parallel to thickness
  • Compressive Strength, 24 hrs at 1010°C, parallel to thickness
  • Compressive Strength, parallel to thickness
  • Volume Resistivity, ASTM D257
  • Surface Resistance, ASTM D257
  • Dielectric Strength, ASTM D149
  • Arc Resistance, ASTM D495
  • CTE, linear
  • Thermal Conductivity, parallel to thickness
  • Thermal Conductivity, parallel to thickness
  • Thermal Conductivity, parallel to thickness
  • Thermal Conductivity, parallel to thickness
  • Melting Point
  • Maximum Service Temperature, Air
  • Shrinkage, perpendicular to thickness
  • Al2O3
  • B2O3
  • CaO
  • MgO
  • Other
  • SiO2
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Zircar Refractory Composites, Inc.

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

New MatWeb Services
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.