MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Vibrantz Technologies IP 745 Passivation Glasses (Pb-B-Si-Al; Pb-Si-Al; Si-Pb-Al Silicates)
Categories: Ceramic; Glass; Oxide; Silicon Oxide

Material Notes: Glass Type: Pb-B-Si-Al
Typical Powder Form: TF, REG, RWG, SRRG

Ferro's passivation glasses are designed for use on transistors, thyristors, and diodes. These products are formulated and produced to achieve very low alkali and iron levels and can be applied by a variety of techniques including photo-spin, spin coat, doctor blading, sedimentation, screen printing, and electrophoresis. IP 745 is primarily used for low-voltage rectifiers using glass bead diode application methods.

Information provided by Ferro Corporation

Ferro Corporation is now a part of Vibrantz Technologies.

Vendors:
Available Properties
  • Density
  • Particle Size, 50% of particles, (SRRG Powder)
  • Particle Size, 50% of particles, (RWG Powder)
  • Particle Size, 50% of particles, (REG Powder)
  • Particle Size, 50% of particles, (TF Powder)
  • Particle Size, SRRG Powder
  • Particle Size, RWG Powder
  • Particle Size, REG Powder
  • Particle Size, TF Powder
  • Ionic Impurities - Na (Sodium), TF, REG Powders
  • Ionic Impurities - Na (Sodium), RWG, SRRG Powders
  • Ionic Impurities - K (Potassium), TF, REG Powders
  • Ionic Impurities - K (Potassium), RWG, SRRG Powders
  • CTE, linear
  • Softening Point
  • Transformation Temperature
  • Processing Temperature, Maximum Junction Temperature
  • Processing Temperature, Typical Firing Temperature; Typical Firing Time: 10-15 min. at Peak
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Vibrantz Technologies, former Ferro Corporation

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

New MatWeb Services
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.