MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Total 3355Z Polypropylene, Oriented Film Extrusion Grade  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polypropylene (PP); Polypropylene, Film Grade

Material Notes: Improved color Homopolymer film grade

Low Residuals - Fina 3355Z utilizes the new Fina proprietary process technology to provide extremely low residuals for improved stability and clarity.

Antistat - Fina 3355Z is formulated to contain an antistat additive for improved film processing in high speed packaging applications.

Slip/Antiblock - Fina 3355Z is available with custom slip and antiblock packages.

FDA - Fina 3355Z complies with all applicable FDA regulations and may be used under these provisions for food contact packaging.

Recommended Applications - Fina 3355Z is recommended in orientation processes for manufacture of specialty packaging films.

Processing - Fina 3355Z resin processes on cast and oriented film extrusion equipment with typical melt temperatures of 450°F-500°F (232°C-260°C).

Data provided by the manufacturer, Total Petrochemicals.

Total Petrochemicals includes former Fina and Atofina plastics product lines.

Vendors:
Available Properties
  • Density, ASTM D1505
  • Water Vapor Transmission, ASTM E96, 90% RH; thickness not specified
  • Melt Flow, ASTM D1238L
  • Film Elongation at Break, MD, ASTM D882
  • Film Elongation at Break, TD, ASTM D882
  • Secant Modulus, MD, ASTM D882
  • Secant Modulus, TD, ASTM D882
  • Film Tensile Strength at Break, MD, ASTM D882
  • Film Tensile Strength at Break, TD, ASTM D882
  • Melting Point, DSC
  • Haze, ASTM D1003
  • Gloss, 45°; ASTM D2457
  • Melt Temperature, oriented film extrusion
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Total Atofina

Category Notes
Plastic

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.