MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Chase Electronic Coatings HumiSeal® 1R32A-2 Acrylic Conformal Coating
Categories: Polymer; Thermoset

Material Notes: HumiSeal® 1R32A-2 is a fast drying, single component acrylic coating, formulated for improved adhesion to typical substrates while providing excellent moisture and environmental protection for printed circuit assemblies. HumiSeal® 1R32A-2 fluoresces under UV light for ease of inspection and is easily repaired. HumiSeal® 1R32A-2 is in full compliance with IPC-CC-830 and the RoHS Directive 2002/95/EC, and is recognized under UL File Number E105698.

Information provided by Chase Electronic Coatings.

Vendors:
Available Properties
  • Density, ASTM D1475
  • Solids Content, Fed-Std-141, Meth. 4044, ± 3%. By weight
  • Volatile Organic Compounds (VOC) Content
  • Viscosity, Fed-Std-141, Meth. 4287
  • Thickness, Recommended coating
  • Modulus of Elasticity, DMA
  • Modulus of Elasticity, DMA
  • Modulus of Elasticity, DMA
  • Insulation Resistance, MIL-I-46058C, Moisture
  • Insulation Resistance, MIL-I-46058C
  • Dielectric Constant, ASTM D150-98
  • Dielectric Breakdown, ASTM D149
  • Dissipation Factor, ASTM D150-98
  • CTE, linear, Below Tg; TMA
  • CTE, linear, Above Tg; TMA
  • Glass Transition Temp, Tg, DSC
  • Flammability, UL94
  • Cure Time, Option
  • Cure Time, Option
  • Cure Time, Optimum Properties
  • Tack-Free Time, Fed-Std-141, Meth. 4061, To handle
  • Shelf Life, DOM
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.