| Random copolymer, Drug Master File (DMF) listed, USP Class VI certified, and FDA compliant Features: Radiation resistant and good contact clarity. Applications: Injection molding: radiation sterilizable medical devices and lab ware. FDA Notes: 21 CFR 177.1520 (c)3.1 Former Huntsman polypropylene products are now produced by Flint Hills Resources. |