  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Eastman Neostar FN007 Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyester TPE; Polyester, TP

Material Notes: Neostar FN007 elastomer is the third in Eastman’s series of tough, clear, durable copolyester ethers. Though originally designed for use in the profile and automotive markets, this innovative copolymer has also found use in tubing and packaging applications. Its excellent chemical, heat, and puncture resistance combined with its strength and durability make it a good choice for applications that require flex-crack resistance and a general utility in harsh environments. Neostar FN007 can be injection molded, extruded in blown film or tubing, or extrusion blow molded. The target inherent viscosity of this product is 1.23.

Applications/Uses

  • Automotive
  • Flexible hinges
  • Pricing channels
  • Retail pricing fins
  • Driver and passenger side air bags
  • Packaging
  • Profiles
  • Tubing
  • Key Attributes

  • Environmentally preferred, non-halogenated material
  • Excellent chemical resistance
  • Exceptional heat resistance and high temperature dimensional stability
  • High flexibility without plasticizers
  • Solvent bondable
  • Vendors:
    Available Properties
    • Specific Gravity, ASTM D792
    • Water Absorption, ASTM D570, 24h Immersion
    • Viscosity Measurement, EMN-A-AC-G-V-1, Inherent
    • Melt Flow, ASTM D1238
    • Hardness, Shore A, ASTM D2240
    • Hardness, Shore D, ASTM D2240
    • Tensile Strength at Break, ASTM D638
    • Tensile Strength, Yield, ASTM D638
    • Elongation at Break, ASTM D638
    • Elongation at Yield, ASTM D638
    • Tensile Modulus, ASTM D638
    • Flexural Modulus, ASTM D790
    • Izod Impact, Notched, ASTM D256
    • Tear Strength, Total, ASTM D1004
    • Heat of Fusion, ASTM E793
    • CTE, linear, ASTM D696
    • Specific Heat Capacity, DSC
    • Specific Heat Capacity, DSC
    • Specific Heat Capacity, DSC
    • Specific Heat Capacity, DSC, solid
    • Specific Heat Capacity, DSC, melt
    • Specific Heat Capacity, DSC, transition
    • Thermal Conductivity, ASTM C177
    • Melting Point, ASTM D3418, Crystalline Peak
    • Crystallization Temperature, DSC, on cooling
    • Vicat Softening Point, ASTM D1525, 1kg load
    • Brittleness Temperature, ASTM D746
    • Glass Transition Temp, Tg, DSC
    • Clash Berg Stiffness Temperature, ASTM D1043, at 930 MPa
    • Clash Berg Stiffness Temperature, ASTM D1043, at 240 MPa
      
    Property Data

    This page displays only the text
    of a material data sheet.

    To see MatWeb's complete data
    sheet for this material (including
    material property data, metal
    compositions, material suppliers,
    etc
    ), please click the button below.

    Manufacturer Notes:
    Eastman Chemical Company

    Category Notes
    Plastic
    Thermoplastic Elastomer

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

     

    Elmet Technologies
    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.