MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
CIP Composites 100 Series Laminated Polymer Bearing Material
Categories: Polymer; Thermoset

Material Notes: The 100 series consists of polyester fabric and one of several solid lubricants (optional) in a resin matrix. Non-metallic, high load, high impact and self lubricating laminated material. Laminated polymer material made by impregnating textile with a thermoset resin. CIP Composites™ offer design engineers an attractive, cost effective alternative to the traditional materials used for bushings, bearings, wear pads, and thrust washers, such as bronze, brass or nylon. CIP Composites™ are only 1/6 the weight of steel, easily machined, have good dimensional stability and do not contain harmful or toxic materials.

Vendors:
Available Properties
  • Density
  • Moisture Absorption, water swell < 0.15%
  • Hardness, Rockwell M, ASTM D785
  • Tensile Strength, ASTM D638
  • Tensile Modulus, ASTM D638
  • Flexural Modulus, ASTM D790
  • Compressive Yield Strength, ASTM D695
  • Compressive Strength, ASTM D695, Parallel to Laminate
  • Compressive Strength, ASTM D695
  • Compressive Modulus, ASTM D695
  • Poissons Ratio, ASTM D3039-08
  • Shear Strength, ASTM D3846
  • Coefficient of Friction, Dynamic, Dry, Grade CIP 151 (MoS2 + PTFE Filled)
  • Coefficient of Friction, Dynamic, Dry, Grade CIP 121 (Graphite Filled)
  • Volume Resistivity, ASTM D257-07
  • Dielectric Strength, ASTM D149-97a
  • CTE, linear, Parallel to Flow, Parallel to Laminate
  • CTE, linear, Transverse to Flow, Normal to Laminate
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Columbia Industrial Products (CIP) Composites

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.