MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Chemically Resistant adhesives
Lord Adhesives CoolTherm™ EP-6037/6010 Epoxy Resin/Hardener Mix
Categories: Polymer; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: LORD CoolTherm™ EP-6037/6010 epoxy system is a two-component epoxy system primarily used by the semiconductor industry to form thermally conductive joints in fabricated heat sinks and between heat sinks and power devices. CoolTherm EP-6037/6010 epoxy system can also be used for bonding semiconductors and transistors to heat sinks, and for general purpose bonding of electronic components.

Features: exhibits low shrinkage and stress on components as it cures. provides a strong adhesion bond to a wide variety of substrates. minimizes the possibility of cracking during severe temperature cycling.

All information provided by Lord.

Vendors:
Available Properties
  • Specific Gravity, EP-6010 Hardener
  • Specific Gravity, EP-6037 Epoxy Resin
  • Water Absorption, EP-6037 Resin mixed with EP-6010 Hardener
  • Viscosity, EP-6010 Hardener
  • Viscosity, EP-6037 Epoxy Resin
  • Hardness, Shore D, EP-6037 Resin mixed with EP-6010 Hardener
  • Tensile Strength, EP-6037 Resin mixed with EP-6010 Hardener
  • Elongation at Break, EP-6037 Resin mixed with EP-6010 Hardener
  • Shear Strength, Lap Shear, aluminum to aluminum, 1" overlap, EP-6037 Resin mixed with EP-6010 Hardener
  • Volume Resistivity, cured, with either EP-6010 Hardener or EP-6252 Hardener
  • Dielectric Strength, cured, with either EP-6010 Hardener or EP-6252 Hardener
  • CTE, linear, EP-6037 Resin mixed with EP-6010 Hardener
  • Thermal Conductivity, EP-6037 Resin mixed with EP-6010 Hardener
  • Glass Transition Temp, Tg, by TMA, EP-6037 Resin mixed with EP-6010 Hardener
  • Cure Time, EP-6037 Resin mixed with EP-6010 Hardener
  • Cure Time, EP-6037 Resin mixed with EP-6010 Hardener
  • Working Life, Working life, resin mixed with EP-6010 Hardener
  • Shelf Life, EP-6037 Resin, from date of manufacture when stored in original, unopened container
  • Shelf Life, EP-6010 Hardener, from date of manufacture when stored in original, unopened container
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Chemically Resistant adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.