| Molecular Formula: C13 H13 N3 Properties : Without odor and poison. Specific gravity : 1.08-1.19. Easily soluble in carbon tetrachloride; Insoluble in water and gasoline. Application : Generally used for natural and synthetic rubbers. Mainly used in manufacture of tires, rubber boards, rubber shoes and other technical rubber goods. Information provided by Ganpati Exim PVT. LTD. |