MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Zircar Zirconia ZYF-50 Zirconia Felt Insulation
Categories: Ceramic; Machinable Ceramic; Oxide; Zirconium Oxide

Material Notes: Zirconia Felt is a true ceramic textile formed by the unique ZIRCAR process for replicating organic structures in inorganic materials. The zirconia felt structure is a ‘needled felt’ which retains its fibrous nature to 2480°C. The stabilized zirconia composition permits the advantages of fibrous insulations to be extended into temperature regions well above the melting temperatures of siliceous and alumina insulation materials.

Zirconia Felt Types ZYF-50, ZYF-100, and ZYF-150 are composed of 100%, 4-6 micron diameter, yttria-stabilized zirconia fibers which are mechanically interlocked. Designed for use in extremely corrosive environments and high temperatures, these felts are 100% inorganic fibers and contain no binders. They undergo no phase transitions on temperature cycling and are very effective thermal insulators, capable of use at temperatures in excess of 1930°C. These materials are equally useful in strong oxidizing and reducing environments, are not reactive to alkali vapors, salts or strong hot solutions. The felts are not wet by most molten metals and have low adsorption surface area and vapor pressure, resulting in low outgassing and contamination in ultra high temperature uses. Zirconia felts are light weight and very porous. They can be surface coated with polymers, filled with inorganic powders or treated with inorganic colloids to achieve special properties.

Features:

  • Low Thermal Conductivity
  • High Porosity
  • High Purity
  • Extreme High Temperature Stability
  • Fibers Stabilized with ~10 wt% Yttria
  • Custom Fillers and Coatings Available
  • Can be Cemented with Zircar Zirconia Cement Type ZR-CEM
  • Can be Rigidized with Zircar Zirconia Rigidizer Type ZIR-RIG
  • Easily Cut to Size
  • Available “Off the Shelf”

Application Information:

  • Zirconia Felt Type ZYF is widely used in crystal growing applications. In the Czochralski method of oxide crystal growing, an iridium crucible is often used to contain the melt. Iridium, a precious metal in the platinum group, vaporizes at high temperature. ZYF acts as thermal insulation and a cushioning barrier as well as a platform for iridium recovery. A layer of ZYF wrapped around the iridium crucible creates a physical barrier between the fragile crucible and the back up insulation. The steep thermal gradient across the ZYF causes condensation of the iridium into the felt from which it can then be easily segregated and recovered.
  • Zirconia Felt Type ZYF is used as an electrolytic cell separators in batteries and fuel cells using alkali electrolytes. Type ZYF is unaffected by long term exposure to KOH.
  • ZYF Felts are used as setter material for powder metal sintering in both vacuum and hydrogen atmospheres.
  • ZYF Felts are used as setter material in contact with quartz glass in melting and hotworking operations.
  • Vacuum furnace and hot isostatic press makers have used ZYF-50 and ZYF-100 as insulation between layers of refractory metal heat shields to improve their insulation package performance.

Information provided by Zircar Zirconia.

Key Words: ZrO2, zirconium oxide
Vendors:
Available Properties
  • Bulk Density
  • Porosity, Bulk
  • Thickness
  • Vapor Pressure
  • Compressive Yield Strength, At 10% compression
  • Specific Heat Capacity
  • Specific Heat Capacity
  • Melting Point
  • Shrinkage, 1 hour isothermal soak at 3000°F
  • Al2O3
  • HfO2
  • SiO2
  • ZrO2+Y2O3
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

New MatWeb Services
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.