Hifax TRC 481P C13097 is a 22% talc filled PP copolymer, with superior flowability, excellent impact/stiffness balance, good processability and good UV resistance. Product is available as a customized color matched, pellet form. This grade is delivered in Black color version. Availability: Europe Application: Exterior Automotive Applications Market: Automotive Processing Method: Injection Molding Attribute: Fast Cycle (Production); Good Dimensional Stability; Good Processability; Good Surface Finish; Good UV Resistance; High Flow; High Impact Resistance Information provided by LyondellBasell. |