MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Chemically Resistant adhesives
3D Systems LaserForm® Ni625 (B), AFTER STRESS RELIEF Nickel Super Alloy
Categories: Metal; 3D Printing/Additive Manufacturing Metal; Ferrous Metal; Tool Steel

Material Notes: Ni625 fine-tuned for use with ProX® DMP 200 metal printers producing industrial parts with high heat resistance, high strength and high corrosion resistance. LaserForm Ni625 (B) is especially resistant to crevice and pitting corrosion. LaserForm Ni625 (B) is formulated and fine-tuned specifically for 3D Systems DMP 200 metal 3D Printers to deliver high part quality and consistent part properties.

Ni625 is known for its combination of high strength and excellent corrosion resistance. LaserForm Ni625 (B) is used where these two attributes need to come together: chemical, marine, aerospace and nuclear industry. Applications include: reaction vessels, tubing, heat exchangers, valves, engine exhaust systems, turbine seals, propeller blades, submarine fittings, propulsion motors, reactor core and control-rod components in nuclear water reactors.

Classification: The chemical composition of LaserForm Ni625 (B) corresponds to ASTM F3056, UNS N06625, Werkstoff Nr. 2.4856, DIN NiCr22Mo9Nb and AMS 5666.

Information provided by 3D Systems

Key Words: ASTM F3056, UNS N06625, Werkstoff Nr. 2.4856, DIN NiCr22Mo9Nb and AMS 5666
Vendors:
Available Properties
  • Density, Absolute theoretical
  • Hardness, Rockwell C, ISO 6508-1
  • Tensile Strength, Ultimate, ASTM E8M, Vertical direction - Z
  • Tensile Strength, Ultimate, ASTM E8M, Horizontal direction - XY
  • Tensile Strength, Yield, ASTM E8M, Rp0.2%, Vertical direction - Z
  • Tensile Strength, Yield, ASTM E8M, Rp0.2%, Horizontal direction - XY
  • Elongation at Break, ASTM E8M, Horizontal direction - XY
  • Elongation at Break, ASTM E8M, Vertical direction - Z
  • Reduction of Area, ASTM E8M, Horizontal direction - XY
  • Reduction of Area, ASTM E8M, Vertical direction - Z
  • Tensile Modulus, ASTM E8M, Youngs, Vertical direction - Z
  • Tensile Modulus, ASTM E8M, Youngs, Horizontal direction — XY
  • CTE, linear
  • Thermal Conductivity
  • Melting Point
  • Aluminum, Al
  • Carbon, C
  • Cobalt, Co
  • Manganese, Mn
  • Molybdenum, Mo
  • Nickel, Ni, Balance
  • Niobium, Nb (Columbium, Cb)
  • Phosphorus, P
  • Silicon, Si
  • Sulfur, S
  • Titanium, Ti
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
3D Systems Corporation

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Chemically Resistant adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.