MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Specialty Compounds RTP Company
Dow 334.03 Performance Polypropylene Polymer  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Blow Molding Grade; Polypropylene, Extrusion Grade; Polypropylene, Impact Modified; Molded/Extruded

Material Notes: DOW D 334.03 Developmental Performance Polypropylene Resin is a propylene-based resin intended for use in extrusion blow molded containers requiring improved impact resistance. Targeted end-use applications include food packaging and household and industrial chemicals.

    Main Characteristics
  • Excellent balance of clarity and toughness
  • Superior toughness versus polypropylene random copolymers
  • Optics (clarity) similar to clarified random copolymer
  • Blush (stress whitening) resistant
  • Complies with U.S. FDA 21 CFR 177.1520(c)
  • This product may be used to produce articles or components of articles used in contact with all food types under Conditions of Use A through H as described in Table 2 of 21 CRF 176.170(c)

Braskem acquired Dow's polypropylene business. This specific grade was discontinued priot to the acquisition and so is listed as a discontinued Dow product.

Vendors:
Available Properties
  • Density, ASTM D792
  • Melt Index of Compound, ASTM D1238
  • Hardness, Shore D, ASTM D2240
  • Tensile Strength, Yield, ASTM D638
  • Elongation at Yield, ASTM D638
  • Flexural Modulus, 1% Secant, ASTM D790A
  • Izod Impact, Notched, ASTM D256A
  • Izod Impact, Notched, ASTM D256A
  • Gardner Impact, ASTM D5420
  • Gardner Impact, ASTM D5420, 23
  • Deflection Temperature at 0.46 MPa (66 psi), ASTM D648, Unannealed
  • Haze, ASTM D1003
  • Haze, ASTM D1003
  • FDA, See notes for details.
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Dow Chemical

Category Notes
Plastic

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Master Bond adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.