MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Metal adhesives
CHT Group EP WQS EPI Engineered Polymers Water Base Quick Set Epoxy
Categories: Polymer; Adhesive; Thermoset; Epoxy

Material Notes: EP WQS Water Base Quick Set, “Powered by Reactamine® Technology”, is a two component 60% solids, no VOC, self-leveling modified epoxy. This versatile new generation epoxy displays low blush, fast cure times, and excellent adhesion characteristics. EP WQS can be used as a surface tolerant primer, and will cure in a variety of harsh situations including high humidity. EP WQS can be applied at temperatures ranging from 40° F to 120° F. This environmentally friendly epoxy displays excellent chemical resistance, water insensitivity, and UV resistance. EP WQS will provide a glossy smooth finish when fully cured. Aggregate can be broadcast into this self-leveling material to provide a non-skid surface. EP WQS emits virtually no odors and can be applied indoors with minimal disturbance contributed to high VOC levels found in most epoxies and polyurethanes.

ApplicationsEP WQS adheres well to several substrates including concrete, steel, and wood. Some typical uses include:

  • CHEMICAL RESISTANT SECONDARY CONTAINMENT
  • OFFSHORE PLATFORMS
  • MAINTENANCE FACILITIES
  • PRIMER FOR MOST POLYUREAS/POLYURETHANES
  • USDA AND FDA ACCEPTABLE COATING
  • INDUSTRIAL FLOORING
  • TANK COATING
  • Part of the Amber Chemical Group. Data provided by manufacturer.

    Formerly Amber Chemical Co (ACC Silicones), aquired by CHT in 2017

    Vendors:
    Available Properties
    • Viscosity, Hardener
    • Viscosity, Resin
    • Hardness, Shore D, ASTM D2240
    • Tensile Strength, ASTM D638
    • Elongation at Break, ASTM D638
    • Flexural Strength, ASTM D790
    • Flexural Modulus, ASTM D638
    • Adhesive Bond Strength, ASTM D4541 Elcometer, Wood (no primer), Delamination
    • Adhesive Bond Strength, ASTM D4541 Elcometer, Concrete (no primer), Concrete Failure
    • Adhesive Bond Strength, ASTM D4541 Elcometer, Steel (no primer), Substrate Failure
    • Izod Impact, Notched, ASTM D628
    • Taber Abrasion, mg/1000 Cycles, ASTM D4060, CS17 Wheel, 1kg
    • Tack-Free Time
    • Pot Life
    • USDA
      
    Property Data

    This page displays only the text
    of a material data sheet.

    To see MatWeb's complete data
    sheet for this material (including
    material property data, metal
    compositions, material suppliers,
    etc
    ), please click the button below.

    Manufacturer Notes:
    none

    Category Notes
    Plastic

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

     

    Metal adhesives
    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.