| MPC-W44C is one of our polyurethane gel formulations specifically designed for padding and cushioning application that requires Shore Durometer OOO scale hardness. With this material, the user can obtain materials with good rebound characteristics and gradual compression deflection rates at the Shore OOO hardness range. This material contains bio-based renewable raw material. The concentration of the renewable material can be above 40% by weight depending on the mixing ratio. This may be classified as bio-based material in some applications. The material does not contain any plasticizer, which is known to leach out to have adverse effects on the plastic film encapsulation materials used in conjunction with the polyurethane gel materials. Like other polyurethane gel formulations, this material is made in such a way that the user can change the hardness and other physical properties of cured part simply by changing the mixing ratio of the given components. This allows users to make various products with just one combination of part-A and part-B components. The applications for this material include cushioning and padding parts for cushioning/padding application, fiber optic cable encapsulation, novelty products, and many more. System Code: MPC-W44C Part-A: MPC-026 (Isocyanate Prepolymer) Part-B: CPC-053 (Curative/ Polyol Blend) Information provided by Northstar Polymers |