MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
SABIC LNP™ LUBRICOMP™ Compound UFL36AS Polyphthalamide (PPA)
Categories: Polymer; Thermoplastic; Polyphthalamide (PPA)

Material Notes: LNP LUBRICOMP UFL36AS compound is based on Polyphthalamide (PPA) resin containing 30% glass fiber, 15% PTFE. Added features of this grade include: Heat Stabilized, Internally Lubricated, Wear Resistant.

Features: Internally Lubricated,Wear resistant,Heat Stabilized,Structural

Information provided by SABIC

Vendors:
Available Properties
  • Specific Gravity, ASTM D792
  • Density, ISO 1183
  • Water Absorption, ASTM D570
  • Water Absorption, ISO 62-1
  • Moisture Absorption, ASTM D570, 23°C/50% RH/24 hrs
  • Moisture Absorption, ISO 62, 23°C / 50% RH
  • Moisture Absorption, Injection Molding
  • Viscosity, ISO 1133, MVR cc/10 min
  • Linear Mold Shrinkage, Flow, SABIC method
  • Linear Mold Shrinkage, Transverse, SABIC method
  • Melt Flow, ASTM D1238
  • Tensile Strength at Break, ISO 527, 5 mm/min
  • Tensile Strength at Break, ASTM D638, 5 mm/min
  • Elongation at Break, ASTM D638, 5 mm/min
  • Elongation at Break, ISO 527, 5 mm/min
  • Tensile Modulus, ASTM D638, 5 mm/min
  • Tensile Modulus, ISO 527, 1 mm/min
  • Flexural Strength, ASTM D790, 1.3 mm/min, 50 mm span
  • Flexural Strength, ISO 178, yield, 2 mm/min
  • Flexural Strength, ISO 178, yield, 2 mm/min
  • Flexural Strength, ISO 178, yield, 2 mm/min
  • Flexural Strength, ISO 178, yield, 2 mm/min
  • Flexural Strength, ISO 178, yield, 2 mm/min
  • Flexural Strength, ISO 178, yield, 2 mm/min
  • Flexural Strength, ISO 178, yield, 2 mm/min
  • Flexural Modulus, ASTM D790, 1.3 mm/min, 50 mm span
  • Flexural Modulus, ISO 178, 2 mm/min
  • Flexural Modulus, ISO 178, 2 mm/min
  • Flexural Modulus, ISO 178, 2 mm/min
  • Flexural Modulus, ISO 178, 2 mm/min
  • Flexural Modulus, ISO 178, 2 mm/min
  • Flexural Modulus, ISO 178, 2 mm/min
  • Flexural Modulus, ISO 178, 2 mm/min
  • Flexural Strain at Break, ISO 178, 2 mm/min
  • Flexural Strain at Break, ISO 178, 2 mm/min
  • Flexural Strain at Break, ISO 178, 2 mm/min
  • Flexural Strain at Break, ISO 178, 2 mm/min
  • Flexural Strain at Break, ISO 178, 2 mm/min
  • Flexural Strain at Break, ISO 178, 2 mm/min
  • Flexural Strain at Break, ISO 178, 2 mm/min
  • Izod Impact Notched, ASTM D256
  • Izod Impact, Unnotched, ASTM D4812
  • Izod Impact, Notched (ISO), ISO 180/1A, 80*10*4
  • Izod Impact, Notched (ISO), ISO 180/1A, 80*10*3
  • Izod Impact, Unnotched (ISO), ISO 180/1U, 80*10*4
  • Izod Impact, Unnotched (ISO), ISO 180/1U, 80*10*4
  • Charpy Impact Unnotched, ISO 179/1eU, Edgew 80*10*4 sp=62mm
  • Charpy Impact, Notched, ISO 179/1eA, Edgew 80*10*4 sp=62mm
  • Dart Drop, Total Energy, ASTM D3763
  • Coefficient of Friction, Dynamic, ASTM D3702 Modified: Manual
  • Coefficient of Friction, Static, ASTM D3702 Modified: Manual
  • K (wear) Factor, ASTM D3702 Modified: Manual, Washer
  • CTE, linear, Parallel to Flow, ASTM D696
  • CTE, linear, Parallel to Flow, ISO 11359-2
  • CTE, linear, Transverse to Flow, ASTM D696
  • CTE, linear, Transverse to Flow, ISO 11359-2
  • Specific Heat Capacity, ASTM E1269
  • Thermal Conductivity, ASTM D5930
  • Deflection Temperature at 0.46 MPa (66 psi), ISO 75/Bf, Flatw 80*10*4 sp=64mm
  • Deflection Temperature at 1.8 MPa (264 psi), ISO 75/Af, Flatw 80*10*4 sp=64mm
  • Deflection Temperature at 1.8 MPa (264 psi), ASTM D648, unannealed
  • Vicat Softening Point, ISO 306, Rate B/120
  • Vicat Softening Point, ISO 306, Rate B/50
  • Vicat Softening Point, ASTM D1525, Rate B/50
  • Zone 2
  • Zone 3
  • Melt Temperature, Injection Molding
  • Mold Temperature
  • Drying Temperature, Injection Molding
  • Dry Time, Injection Molding
  • Back Pressure
  • Screw Speed
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Saudi Basic Industries Corporation; SABIC Innovative Plastics (GE Plastics)

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.