MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Online Metals
Visit Online Metals for fast service
on small quantity orders.
ExxonMobil EXACT™ 0210 Ethylene-based Plastomer for Multilayer Film Applications  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Elastomer, TPE

Material Notes: Exact 0210 plastomer is an ethylene octene copolymer produced using ExxonMobil Chemical's EXXPOL™ Technology. It is designed for seal layers in multilayer film applications requiring good flow/caulking and low SIT.

Key Features:

  • Low temperature heat seal performance including low seal initiation temperature and good caulking/flow.
  • Superior toughness and tear strength.
  • High clarity and low fogging tendency.
  • High filler and oil acceptance.
  • Low hexane extractables
Availability: Africa & Middle East, Europe, North America, Asia Pacific, Latin America and South America

Additive: Thermal Stabilizer

This polymer complies with FDA regulation 21 CFR 177.1520 (Olefin polymers), paragraph (c) 3.2c, and may be used as articles or components of articles intended for use in contact with food, except for articles used for packing or holding food during cooking. Finished articles may contact food only under Conditions of Use C through H described in Table 2 of 21 CFR 176.170(c).

Information provided by ExxonMobil Chemical

Vendors:
Available Properties
  • Density, ISO 1183
  • Melt Flow, ISO 1133
  • Hardness, Shore D, ISO 868
  • Melting Point, ISO 11357-3, Peak Melting Temperature
  • Vicat Softening Point, ISO 306/A
  • Brittleness Temperature, ASTM D746
  • FDA
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Exxon Chemical

Category Notes
Plastic
Thermoplastic Elastomer

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2026 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.