Sterilization: Gamma radiation, EtO, and E-beam
Applications: Syringes, medical device components
Regulatory: FDA – 21 CFR 177.1520(c) 3.1a; USP <88> Class VI, USP<85>, and ISO 10993-5
This page displays only the textof a material data sheet.To see MatWeb's complete datasheet for this material (includingmaterial property data, metalcompositions, material suppliers,etc), please click the button below.
Category NotesPlastic