MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
ChevronTexaco Texcool® P-155
Categories: Fluid

Material Notes: In service Texaco Texcool P 150 provides:
  • Silicate free
  • Excellent heat transfer properties
  • Superior antifoam characteristics
  • Superior corrosion protection for brass, copper, solder, steel and cast iron
  • Borax-free for maximum aluminum protection
  • Nitrite-free, amine-free
  • Mixes readily with clean tap water
  • Compatible with cooling system filters
  • Compatible with heavy duty diesel supplemental coolant additives
  • 100% biodegradable in its pure unused form

Texaco Texcool P 155 is a 50 volume % mixture of Texaco Texcool P 150 and 50 volume % deionized water.

Texaco Texcool P 150 is a single phase, propylene glycol based product blended with a premium quality additive package. It is a silicate free coolant designed for use in stationary engines. This product provides antifoam properties, and rust and corrosion protection for brass, copper, solder, steel and cast iron. It mixes readily with clean tap water and is compatible with cooling system filters and supplemental additives.

Texaco Texcool P 150 is free of nitrites and amines.

Texaco Texcool P 150 is an inhibited propylene glycol used as a heavy duty industrial coolant and heat transfer agent. The inhibitor system is designed to protect brass, copper, solder, steel, cast iron, aluminum, and other metals commonly found in industrial cooling and heating systems. A foam inhibitor is included to minimize foaming tendencies during service.

Texaco Texcool P 150 coolant is recommended as a coolant in stationary engines, in applications such as natural gas processing, irrigation, power generating systems, oil field operations, and portable air compressors. Texaco Texcool P 150 should not be used in automotive or nonstationary heavy duty diesel applications! Texaco Texcool P 150 coolant protects the cooling system from freezing in winter, overheating in summer, and corrosion in all seasons. Extensive simulated service and actual service tests have proven the effectiveness of Texaco Texcool P 150 coolant in heat transfer applications over the use of brine or uninhibited glycol-water solutions. The results were lower maintenance costs and improved heat transfer with Texaco Texcool P 150.

Texaco Texcool P 150 coolant is recommended as a heat transfer fluid for line heaters. A line heater circulates a heated fluid around a pipe to raise the temperature of the pipe content in order to control reactions or ease pumping operations.

Texaco Texcool P 150 coolant is recommended as a heat transfer fluid for snow melting systems, loading ramps, walkways, highways, airfield runways, and as a coolant in ice skating rinks and air conditioning systems.

Note: These products are not to be used to protect the inside of potable water systems against freezing.Texaco Texcool P 150 meets or exceeds the requirements of:

  • Waukesha stationary engines
  • Caterpillar stationary engines
  • Cummins stationary engines

Typical test data are average values only. Minor variations which do not affect product performance are to be expected in normal manufacturing.

Vendors:
Available Properties
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
ChevronTexaco Corp

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

New MatWeb Services
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.