| Plasticized PA12; High viscosity, light and heat stabilized, with lubricant, excellent low temperature impact properties; Designed for injection molding and extrusion, such as air brake and solenoid pipe, vacuum pipe Product ID: 9HD6FGPS Business Unit: Plastics Applications: Vacuum Lines; Solenoid Pipe; Air Brake Information provided by Wanhua Chemical Group Co., Ltd. |