MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Metal adhesives
Resinlab® EP1300 Clear Unfilled Electronic Grade Epoxy Encapsulant
Categories: Polymer; Thermoset; Epoxy; Epoxy Encapsulant, Unreinforced

Material Notes: Resinlab™ EP1300 Clear (Formerly Lab Product W092602) is a two part unfilled electronic grade epoxy encapsulant designed for small to medium sized castings. It has a pot life of about one hour and cures quickly to a tack free handle strength at room temperature within 3 to 4 hours reaching a tough, semi-rigid state within 48 hours. Cure can be accelerated by the addition of heat. Times and temperatures from ½ hour at 100°C to 1 hour at 80°C or 4 hours at 50°C fill bring the product to full cure. It has good wetting and adhesion to most surfaces and is free flowing to penetrate voids and give good air release. It has very good resistance to water, acids and bases and most organic solvents.

Information Provided by Resinlab L.L.C., an Ellsworth Adhesives Company.

Vendors:
Available Properties
  • Specific Gravity, TM R050-16, Part B
  • Specific Gravity, TM R050-16, Mixed
  • Specific Gravity, TM R050-16, Part A
  • Water Absorption, TM R050-35
  • Viscosity, TM R050-12, Part B, RVT, #5, 2.5 rpm
  • Viscosity, TM R050-12, Mixed
  • Viscosity, TM R050-12, Part A, RVT, #6, 2.5 rpm
  • Hardness, Shore D, TM R050-17
  • Tensile Strength at Break, TM R050-36
  • Tensile Strength, Ultimate, TM R050-36
  • Tensile Strength, Yield, TM R050-36
  • Elongation at Break, TM R050-36
  • Tensile Modulus, TM R050-36
  • Compressive Yield Strength, TM R050-38
  • Compressive Strength, TM R050-38, Ultimate
  • Compressive Strength, TM R050-38, Break
  • Compressive Modulus, TM R050-38
  • Adhesive Bond Strength, TM R050-37, Lap shear; 2024 T3 Al Abraded / MEK Wipe
  • Peel Strength, Al to Al
  • Volume Resistivity
  • Dielectric Constant
  • Dielectric Strength
  • CTE, linear, below Tg
  • CTE, linear, above Tg
  • Thermal Conductivity
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Glass Transition Temp, Tg, TM R050-25
  • Transmission, Visible, clear; thickness not quantified
  • Pot Life, TM R050-19, Mass: 100g
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Metal adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.