MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Röchling LAMINEX® 2140 Cotton Fabric, Phenolic Resin Impregnated, MoS2 Filled
Categories: Polymer; Thermoset; Phenolic; Phenolic, Novolac, Fabric Filled

Material Notes: Application: bearing shells and bearing collars

Information provided by Schwartz Technical Plastics GmbH. Schwartz was acquired by Röchling in 2018.

Key Words: PF-7708
Vendors:
Available Properties
  • Density, ISO R 1183
  • Ball Indentation Hardness, ISO 2039; partially, Hc 30
  • Tensile Strength, Yield, ISO-DIS 527
  • Tensile Modulus, DIN 53457
  • Flexural Strength, DIN 54352
  • Compressive Strength, ISO 604
  • Izod Impact, Notched (ISO), DIN 53453
  • Izod Impact Resistance, DIN 53453, swinging hammer 0,1 DIN 51222
  • CTE, linear, DIN 53752
  • Thermal Conductivity, DIN 52612
  • Maximum Service Temperature, Air, Continuous
  • Maximum Service Temperature, Air, Intermittent
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.