| Very good physical and mechanical properties, very good resistance to the temperature till 150° C High resistance to the permanent deformation. Very good oil resistance, mineral/plant and animal fats, to hydrocarbons/petrol , to gas and some freon types SolidCompact rubber has closed cells and density more than 1.00 gr/cm3 Information provided by Eurofoam s.r.l. |