MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Carpenter Custom 630 (17-Cr-4Ni) Precipitation Hardening Stainless Steel, Condition H 900 (Age-Hardened 482°C/1hr/AC)
Categories: Metal; Ferrous Metal; Stainless Steel; Precipitation Hardening Stainless; T S10000 Series Stainless Steel

Material Notes: Data provided by Carpenter Technology Corporation.

Custom 630 (17Cr-4Ni) is a martensitic precipitation/age-hardening stainless steel offering high strength and hardness along with excellent corrosion resistance. It has good fabricating characteristics and can be age hardened by a single-step, low temperature treatment. It has been used for a variety of applications including oil field valve parts, chemical process equipment, aircraft fittings, fasteners, pump shafts, nuclear reactor components, gears, paper mill equipment, missile fittings, and jet engine parts. Project 70® stainless Custom 630 is an improved machinability modification.

Key Words: AISI 630; UNS S17400; 17-4PH, 17/4PH, 17-4 PH, Precipitation Hardening PH Stainless Steel, 17-4
Vendors:
Available Properties
  • Density
  • Hardness, Brinell
  • Hardness, Knoop, Estimated from Rockwell C
  • Hardness, Rockwell C
  • Hardness, Vickers, Estimated from Rockwell C
  • Tensile Strength, Ultimate
  • Tensile Strength, Ultimate
  • Tensile Strength, Ultimate
  • Tensile Strength, Ultimate
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Tensile Strength, Yield
  • Tensile Strength, Yield
  • Tensile Strength, Yield
  • Tensile Strength, Yield
  • Elongation at Break, In 50 mm
  • Elongation at Break, In 50 mm
  • Elongation at Break, In 50 mm
  • Elongation at Break, In 50 mm
  • Elongation at Break
  • Reduction of Area
  • Reduction of Area
  • Reduction of Area
  • Reduction of Area
  • Reduction of Area
  • Modulus of Elasticity
  • Poissons Ratio
  • Shear Modulus, Calculated
  • Charpy Impact, V-notch
  • Electrical Resistivity
  • CTE, linear
  • CTE, linear
  • CTE, linear
  • Specific Heat Capacity, condition H 900
  • Thermal Conductivity, condition H 900
  • Thermal Conductivity, condition H 900
  • Carbon, C
  • Chromium, Cr
  • Copper, Cu
  • Iron, Fe, as remainder
  • Manganese, Mn
  • Nb + Ta
  • Nickel, Ni
  • Niobium, Nb (Columbium, Cb)
  • Phosphorus, P
  • Silicon, Si
  • Sulfur, S
  • Tantalum, Ta
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Carpenter Technology Corporation (Cartech)

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.