MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
SSAB GreenCoat® RWS Pural BT Color Coated Steel
Categories: Metal; Ferrous Metal; Carbon Steel

Material Notes: GreenCoat RWS Pural BT color coated steel is available in matte finish. It provides a coating where rapeseed oil and other renewable raw materials are used. SSAB has long experience of Bio-based Technology (BT) in GreenCoat products. GreenCoat RWS Pural BT offers the highest level of durability for rainwater systems using a double-sided coating (same coating is applied on both sides of the sheet). GreenCoat RWS Pural BT color coated steel provides excellent corrosion resistance (RC5), gloss retention and colorfastness (Ruv5). GreenCoat RWS Pural BT possesses excellent forming properties enabling very demanding folding even down to -15°C, allowing for year round installation at lower costs. Excellent weather resistance together with regular maintenance and the cleaning of rainwater systems can maximize the service life of the product. GreenCoat RWS Pural BT complies with current REACH regulations and is fully chromate-free. SSAB’s color coated steels are all manufactured according to EN 10169. GreenCoat and Pural are trademarks of the SSAB group of companies.

Data provided by SSAB.

Vendors:
Available Properties
  • Thickness, Matt, Coating thickness, nominal (primer + top coat)
  • Thickness, Matt, steel thickness
  • Maximum Service Temperature, Air, Matt
  • Gloss, Matt
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
SSAB Tunnplat AB

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.