MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Phillips 66 Kendall® Air Cooled 2-Cycle Motor Oil SAE Grade 20
Categories: Fluid; Lubricant

Material Notes: Kendall® Air Cooled 2-Cycle Motor Oil is a low-ash engine oil designed primarily for use in small, low-output (less than 50 HP) 2-stroke cycle outboard engines. It also is recommended for use in small air-cooled 2-stroke cycle engines such as those found on lawn mowers, weed trimmers, and leaf blowers. Air Cooled 2-Cycle Motor Oil is formulated with a low-ash, detergent additive package to help minimize engine deposits and reduce spark plug fouling and preignition problems.

Applications:

  • Low-output (less than 50 horsepower) 2-stroke cycle outboard engines
  • Lawn-care equipment (mowers, weed trimmers, leaf blowers)
Air Cooled 2-Cycle Motor Oil meets the requirements of:
  • API Service TC
  • JASO FB
Features/Benefits:
  • Low-ash formulation helps minimize engine deposits and pre-ignition
  • Minimizes piston ring sticking and helps reduce exhaust port blocking
  • Protects against piston and cylinder scuffing
  • Reduces spark plug fouling
  • Protects against rust and corrosion
  • Keeps engine parts clean
  • Dyed for easy visibility when mixed with gasoline

Information provided by Phillips 66 Lubricants.

Vendors:
Available Properties
  • Specific Gravity
  • Density
  • Viscosity Measurement, Index
  • Kinematic Viscosity at 40°C (104°F)
  • Kinematic Viscosity at 100°C (212°F)
  • Ash, ASTM D874, Sulfated
  • Pour Point
  • Flash Point, PMCC
  • Flash Point, COC
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.