MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Chemically Resistant adhesives
Master Bond EP46HT-2AO Black Thermally Conductive, Electrically Insulating Epoxy
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive; Epoxy Encapsulant, Unreinforced; Epoxy, High Temperature

Material Notes: Key Features:
  • Thermally conductive
  • Excellent electrical insulator
  • Long working life
  • Passes NASA low outgassing test requirements
  • Unrivaled dimensional stability
  • Exceptionally high temperature resistance
Product Description: Master Bond EP46HT 2AO Black is a two component epoxy system for demanding bonding, sealing and encapsulation applications where thermal conductivity, electrical insulation and high temperature resistance are required. It is 100% reactive and does not contain any solvents or diluents. EP46HT-2AO Black is formulated to cure rapidly and requires a cure temperature of 250°F or more. An optimal curing schedule is 3-4 hours at 250-300°F followed by a post cure of 2-3 hours at 350-400°F. The glass transition temperature is quite high, exceeding 200°C and the service temperature range is -100°F to +500°F. Once cured, EP46HT-2AO Black features exceptional physical and mechanical properties, along with exquisite dimensional stability. It bonds well to a wide variety of substrates including metals, glass, ceramics, composites, various rubbers and many plastics. It is a highly functional electrical insulator. It has very good chemical resistance to water, fuels, oils, acids and bases. Most importantly, it passes NASA low outgassing testing. The color of Part A is black and Part B is gray. This high powered combination of product properties allows this system to be used in challenging applications in aerospace, electronics, optoelectronics and in vacuum environments.

Product Advantages:

  • Extremely forgiving mix ratio
  • Very long open time at room temperature
  • Top notch heat resistance
  • Noteworthy thermal conductivity combined with fine electrical insulation values
  • High quality dimensional stability
  • Meets NASA low outgassing requirements

Information provided by Master Bond Inc.

Vendors:
Available Properties
  • Viscosity, Part B
  • Viscosity, Part A
  • Viscosity, mixed, thixotropic
  • Hardness, Shore D
  • Tensile Strength
  • Tensile Modulus
  • Compressive Strength
  • Adhesive Bond Strength, Tensile lap, Aluminum to Aluminum
  • Volume Resistivity
  • Dielectric Strength
  • CTE, linear
  • Thermal Conductivity
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Glass Transition Temp, Tg
  • Cure Time, Post cure for optimum properties at 350-400°F
  • Cure Time
  • Working Life, After mixing, 100 g batch
  • Shelf Life, in original, unopened containers
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Master Bond Inc.

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Chemically Resistant adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.