Stanyl CR310 is a special V-0 grade which is mainly based on Nitrogen-based Flame Retardant Technology. It is a .good flowing material which is especially suitable as arc quenching material in circuit breakers.
This page displays only the textof a material data sheet.To see MatWeb's complete datasheet for this material (includingmaterial property data, metalcompositions, material suppliers,etc), please click the button below.
Category NotesPlasticPA, Polyamide