MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Wacker Elastosil® LR 3071/40 A/B Liquid Silicone Rubber
Categories: Polymer; Thermoset; Silicone; Silicone Rubber; Liquid Silicone Rubber (LSR)

Material Notes: Self-adhesive liquid silicone rubbers of the ELASTOSIL® LR 3071 series are paste-like, easily pigmentable two-component compounds with extremely short curing times.

ELASTOSIL® LR 3071 series are primerless, selfbonding grades that adhere to various plastic substrates (e.g. PA, PBT) and metals, but not in the mold (adhesive adherence, protects against loss prior to assembly). The bonding is improved by an ageing process (e.g. one hour at 100°C) or by a longer storing at room temperature. Because of the individual surface properties each substrate must be tested before mass production. If necessary one has to check the development of adhesive properties over time and/or in an environment relevant to the application. The vulcanizates are noted for good mechanical and electrical properties.

Application: ELASTOSIL® LR 3071 series are particularly suitable for the economical production of large series of overmolded parts (thermoplastic/elastomer), even in a comolding process (shuttle mold) under standard conditions, without any special treatment of the mold surface. Parts made from ELASTOSIL® LR 3071 can generally be used for technical applications without postcuring. Postcured parts can be used for food contact applications and are suitable for use under the Recommendation "XV. Silicones" of the BfR and FDA § 177.2600 under observance of any given limitations on extractable and volatile substances.

Information provided by Wacker Chemie AG.

Vendors:
Available Properties
  • Density, ISO 1183-1 A
  • Viscosity, DIN 53019
  • Viscosity, DIN 53019
  • Hardness, Shore A, DIN 53505
  • Tensile Strength at Break, DIN 53504 S 1
  • Elongation at Break, DIN 53504 S 1
  • Tear Strength, ASTM 624 B
  • Compression Set, DIN ISO 815-B
  • Compression Set, DIN ISO 815-B
  • Maximum Service Temperature, Air, with heat stabilizer
  • Minimum Service Temperature, Air
  • Transmission, Visible, "Transparent" but manufacturer does not quantify.
  • Cure Time, in press
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Elmet Technologies
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.