| Available Properties |
|---|
- Specific Gravity, ASTM D792
- Density, ISO 1183
- Water Absorption, Sim. to ISO 62, Dry
- Water Absorption, ASTM D570
- Moisture Absorption, Sim. to ISO 62, Dry
- Viscosity, ASTM D3835, Melt
- Melt Flow, ISO 1133, cm³/10 min Volumetric Rate
- Melt Flow, ASTM D1238
- Hardness, Shore D, ASTM D2240
- Tensile Strength at Break, ASTM D638
- Tensile Strength, Yield, ISO 527-1/-2, Dry
- Tensile Strength, Yield, ASTM D638
- Elongation at Break, ISO 527-1/-2, Dry
- Elongation at Break, ASTM D638
- Elongation at Yield, ASTM D638
- Elongation at Yield, ISO 527-1/-2, Dry
- Tensile Modulus, ISO 527-1/-2, Dry
- Tensile Modulus, ASTM D638
- Flexural Strength, ASTM D790
- Flexural Modulus, ASTM D790
- Compressive Strength, ASTM D695
- Izod Impact, Notched, ASTM D256
- Izod Impact, Unnotched, ASTM D256
- Charpy Impact, Notched, ISO 179/1eA, Dry
- Charpy Impact, Notched, ISO 179/1eA, Dry
- Coefficient of Friction, Dynamic, ASTM D1894, vs. steel
- Coefficient of Friction, Static, ASTM D1894, vs. steel
- Taber Abrasion, mg/1000 Cycles, ASTM-G195-13A, CS 17 1000g:pad
- Volume Resistivity, ASTM D257, 65% R.H
- Volume Resistivity, IEC 60093, Dry
- Surface Resistivity per Square, ASTM D257
- Dielectric Constant, IEC 60250, Dry
- Dielectric Constant, ASTM D150
- Dielectric Constant, IEC 60250, Dry
- Dielectric Strength, ASTM D149
- Dissipation Factor, IEC 60250, Dry
- Dissipation Factor, ASTM D150
- Dissipation Factor, IEC 60250, Dry
- CTE, linear, ASTM D696
- CTE, linear, Parallel to Flow, ISO 11359-1/-2, Dry
- Specific Heat Capacity, DSC
- Thermal Conductivity, ASTM D433
- Melting Point, ASTM D3418
- Melting Point, ISO 11357-1/-3, 10°C/min; Dry
- Maximum Service Temperature, Air, UL RTI
- Deflection Temperature at 0.46 MPa (66 psi), ASTM D648
- Deflection Temperature at 0.46 MPa (66 psi), ISO 75-1/-2, Dry
- Deflection Temperature at 1.8 MPa (264 psi), ASTM D648
- Deflection Temperature at 1.8 MPa (264 psi), ISO 75-1/-2, Dry
- Vicat Softening Point, ISO 306, 50°C/h 50N; Dry
- Glass Transition Temp, Tg, ASTM D7028
- Glass Transition Temp, Tg, ISO 11357-1/-2, 10°C/min; Dry
- Decomposition Temperature, 1% wt. loss, TGA, in air
- Decomposition Temperature, 1% wt. loss, TGA, in nitrogen
- UL RTI, Electrical, UL 746B
- UL RTI, Mechanical without Impact, UL 746B
- Flammability, UL94, IEC 60695-11-10
- Flammability, UL94, IEC 60695-11-10, Yellow Card Available; Dry
- Oxygen Index, ASTM D2863
- Oxygen Index, ISO 4589-1/-2, Dry
- Refractive Index, ASTM D542, sodium D line
- Processing Temperature, ISO 293, Compression Molding; Molding Temperature
|
| | |